Adhesive joints

Dr. Dmitri Kopeliovich

Strength of an adhesive bonding strongly depends on the direction and distribution of the stresses formed in the joint as a result of the loads applied to it.

Typical forces, which may be applied to adhesive joints are presented in the figure below.

Typical_forces.png

Two aderends (substrate) may be bonded by different ways shown in the picture.
Lap and strap joints provide the maximal bonding strength. Butt joint is the weakest joint type.

adhesive_joints.png

Fillet joint imparts additional strength to the adhesive joints.

adhesive_fillets.png|

Basic rules of adhesive joint design:

  • Peeling and cleavage stresses should be minimal;
  • Shear stress is preferrable than tension;
  • Bonding area should be as large as possible;
  • Adhesive layer thickness should be minimal and uniform.


The figure below presents design of several joint types at different loading conditions.

adhesive_joint_design.png

to top


Related internal links

adhesive_joints.txt ยท Last modified: 2023/12/13 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License