| Carbon-Carbon Composite (randomly oriented fibers) | ||||
| Composition: carbon matrix + 40% carbon fibers | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.7 *10³ | kg/m³ | 106 | lb/ft³ | 
|---|---|---|---|---|
| Flexural strength | 250 | MPa | 36300 | psi | 
| Fracture modulus of elasticity | 50 | GPa | 7250 | ksi | 
| Tensile strength | 250 | MPa | 36300 | psi | 