| Low temperature hydraulic oil ISO 22 | ||||
| Mineral based hydraulic oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.864 *10³ | kg/m³ | 53.9 | lb/ft³ | 
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 21.6 | cSt | 21.6 | cSt | 
| Kinematic viscosity at 212°F (100°C) | 4.23 | cSt | 4.23 | cSt | 
| Viscosity index | 99 | 99 | ||
| Flash point | 208 | ºC | 406 | ºF | 
| Pour Point | -36 | ºC | -33 | ºF | 
| Aniline Point | 98 | ºC | 208 | ºF | 
| Color | max. 1.5 | max. 1.5 | ||