Main page
 About us
 Sliding Bearings Consulting
 Advertising Opportunities


to Thermoplastics
 to Properties of polymers
(submitted by the website administration)
 
| Thermoplastic | ||||
| Polyvinylidene fluoride (PVDF) | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.78*10³ | kg/m³ | 111.1 | lb/ft³ | 
|---|---|---|---|---|
| Modulus of elasticity | 1.95 | GPa | 283 | ksi | 
| Tensile strength | 55 | MPa | 8000 | psi | 
| Elongation (max.) | 250 | % | 250 | % | 
| Notched impact strength | 33 | kJ/m2 | 15.7 | ft*lbf/in2 | 
| Hardness | 79 | Shore D | 79 | Shore D | 
| Thermal expansion (20 ºC) | 130*10-6 | ºCˉ¹ | 72*10-6 | in/(in* ºF) | 
| Thermal conductivity | 0.16 | W/(m*K) | 1.11 | BTU*in/(hr*ft²*ºF) | 
| Melting point | 170 | ºC | 338 | ºF | 
| Maximum work temperature | 150 | ºC | 302 | ºF | 
| Dielectric constant | 7 | - | 7 | - | 
| Dielectric strength | 25 | kV/mm | 635 | V/mil | 
| Electrical resistivity | 1.5*1012 | Ohm*m | 1.5*1014 | Ohm*cm | 
Applications: tubes for chemicals, valves, gaskets, pump parts for chemical industry.
 
 to Polymers
 to Thermoplastics
 to Properties of polymers   