| Quenching oil ISO 22 | ||||
| Mineral based oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.865 *10³ | kg/m³ | 54.0 | lb/ft³ | 
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 21.3 | cSt | 21.3 | cSt | 
| Kinematic viscosity at 212°F (100°C) | 4.2 | cSt | 4.2 | cSt | 
| Viscosity index | 100 | 100 | ||
| Flash point | 209 | ºC | 408 | ºF | 
| Pour Point | -18 | ºC | -0.4 | ºF | 
| Color | 0.5 | 0.5 | ||
Applications: general purpose heat treatment, quenching and heat transfer oil.