Property Value in metric unit Value in US unit
Matrix Styrene-DVB, gel
Functional group Quaternary amine
Exchange capacity 1.3 eq/l 28.4 kgr of CaCO3/ft³
Water content 55%
Total swelling (Cl- → OH-) 20%
Mean particle size 0.58 mm 22.8 μinch
Particle density 1.08 kg/l 70.7 lb/ft³
Shipping weight 0.67 kg/l 42 lb/ft³
Maximum work temperature 100 °C 212 °F
PH range 0-14
Min. bed depth 800 mm 2.6 ft
Service flow rate 5-60 m/h 2-24 gpm/ft2
Co-current regeneration rinse 1-10 m/h 0.4-4 gpm/ft2
Counter-current regeneration rinse 5-20 m/h 2-8 gpm/ft2
Total rinse requirement 3-6 bed volumes
Regenerant NaOH (2-5%)

Related internal links

strong_anion_exchange_resin_in_chloride_form.txt · Last modified: 2023/12/14 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License