| Strong Anion Exchange Resin in hydroxide form | ||||
| Uniform Particle Size, High Capacity, Strong Anion Exchange Resin in hydroxide form | ||||
| Property | Value in metric unit | Value in US unit | ||
| Matrix | Styrene-DVB, gel | |||
|---|---|---|---|---|
| Functional group | Quaternary amine | |||
| Exchange capacity | 1.0 | eq/l | 21.9 | kgr of CaCO3/ft³ | 
| Water content | 66% | |||
| Total swelling (Cl- → OH-) | 20% | |||
| Mean particle size | 0.61 | mm | 24.0 | μinch | 
| Particle density | 1.06 | kg/l | 69.4 | lb/ft³ | 
| Shipping weight | 0.64 | kg/l | 40 | lb/ft³ | 
| Maximum work temperature | 60 | °C | 140 | °F | 
| PH range | 0-14 | |||
| Min. bed depth | 800 | mm | 2.6 | ft | 
| Service flow rate | 5-60 | m/h | 2-24 | gpm/ft2 | 
| Co-current regeneration rinse | 1-10 | m/h | 0.4-4 | gpm/ft2 | 
| Counter-current regeneration rinse | 5-20 | m/h | 2-8 | gpm/ft2 | 
| Total rinse requirement | 3-6 bed volumes | |||
| Regenerant | NaOH (2-5%) | |||