| Fluorocarbon solvent Trichlorofluoromethane (Freon 11) | ||||
| Chemical formula: CCl3F | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 77°F (25°C) | 1.494 *10³ | kg/m³ | 93.3 | lb/ft³ | 
|---|---|---|---|---|
| Vapor pressure at 68°F (20°C) | 89 | kPa | 13 | psi | 
| Boiling point | 23.8 | ºC | 74.8 | ºF | 
| Melting Point | -110.5 | ºC | -166.9 | ºF | 