Chemical composition: Si=7.5%, Al balance
Property Value in metric unit Value in US unit
Density 2.68 *10³ kg/m³ 167 lb/ft³
Thermal expansion (20 ºC) 21.6*10-6 ºCˉ¹ 12.0*10-6 in/(in* ºF)
Thermal conductivity 180 W/(m*K) 1250 BTU*in/(hr*ft²*ºF)
Electric resistivity 4.16*10-8 Ohm*m 4.16*10-6 Ohm*cm
Liquidus temperature 613 ºC 1135 ºF
Solidus temperature 577 ºC 1070 ºF