| Chlorinated solvent 1,1,1-trichloroethane (methyl chloroform) | ||||
| Chemical formula: CH3-CCl | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 68°F (20°C) | 1.34*10³ | kg/m³ | 83.6 | lb/ft³ | 
|---|---|---|---|---|
| Viscosity at 68°F (20°C)) | 0.87 | cP | 5.84*10-4 | lb/ft·s | 
| Surface tension at 77°F (25°C) | 0.025 | N/m | 1.43*10-4 | lbf/in | 
| Vapor pressure at 68°F (20°C) | 13300 | Pa | 1.93 | psi | 
| Boiling point | 74 | ºC | 165 | ºF | 
| Melting Point | -30 | ºC | -22 | ºF | 
| Autoignition temperature | 537 | ºC | 999 | ºF | 
| Dielectric constant at 68°F (20°C) | 7.53 | 7.53 | ||
| Specific heat capacity | 926 | J/(kg*K) | 0.221 | BTU/(lb*ºF) | 
| Latent heat of vaporization | 243 | kJ/kg | 104.5 | BTU/lb |