| General purpose cyanoacrylate adhesive | ||||
| Single component moisture activated curing adhesives | ||||
| Property | Value in metric unit | Value in US unit | ||
| Viscosity at 77°F (25°C) | 40 | cP | 8.35*10-4 | lbf*sec/ft² | 
|---|---|---|---|---|
| Fixture time, steel, 77°F (25°C) | 10 | min | 10 | min | 
| Maximum gap | 0.102 | mm | 0.004 | in | 
| Shear strength, steel, 77°F (25°C) | 20 | MPa | 2900 | psi | 
| Min. service temperature | -54 | ºC | -65 | ºF | 
| Max. service temperature | 180 | ºC | 82 | ºF |