to Ceramic Matrix Composites (introduction)
to Properties of composites
(submitted by the website administration)
cg-Nicalon | ||||
Composition: Silicon carbon (SiC) matrix + SiC long (cont.) fibers (14 mkm diameter) | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 2.55 *10³ | kg/m³ | 159 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 195 | GPa | 28300 | ksi |
Tensile strength | 220 | MPa | 31900 | psi |
Thermal expansion (20 ºC) | 3.2*10-6 | ºCˉ¹ | 1.8*10-6 | in/(in* ºF) |
Thermal heat capacity | 630 | J/(kg*K) | 0.15 | BTU/(lb*ºF) |
Thermal conductivity | 1.5 | W/(m*K) | 10.4 | BTU*in/(hr*ft²*ºF) |