| Strong Cation Exchange Resin in hydrogen form | ||||
| Uniform Particle Size, High Capacity Strong Acid Cation Exchange Resin | ||||
| Property | Value in metric unit | Value in US unit | ||
| Matrix | Styrene-DVB, gel | |||
|---|---|---|---|---|
| Functional group | Sulfonic acid | |||
| Exchange capacity | 2 | eq/l | 43.7 | kgr of CaCO3/ft³ | 
| Water content | 45% | |||
| Total swelling (Na+ → H+) | 8% | |||
| Mean particle size | 0.59 | mm | 23.2 | μinch | 
| Particle density | 1.28 | kg/l | 79.9 | lb/ft³ | 
| Shipping weight | 0.82 | kg/l | 51 | lb/ft³ | 
| Maximum work temperature | 120 | °C | 250 | °F | 
| PH range | 0-14 | |||
| Min. bed depth | 800 | mm | 2.6 | ft | 
| Service flow rate | 5-60 | m/h | 2-24 | gpm/ft2 | 
| Co-current regeneration rinse | 1-10 | m/h | 0.4-4 | gpm/ft2 | 
| Counter-current regeneration rinse | 5-20 | m/h | 2-8 | gpm/ft2 | 
| Total rinse requirement | 2-5 bed volumes | |||
| Regenerant | H2SO4 (1-8%) or HCl (4-8%) | |||