| Strong Cation Exchange Resin in sodium form | ||||
| Uniform Particle Size, High Capacity Strong Acid Cation Exchange Resin | ||||
| Property | Value in metric unit | Value in US unit | ||
| Matrix | Styrene-DVB, gel | |||
|---|---|---|---|---|
| Functional group | Sulfonic acid | |||
| Exchange capacity | 1.8 | eq/l | 39.3 | kgr of CaCO3/ft³ | 
| Water content | 53% | |||
| Total swelling (Na+ → H+) | 8% | |||
| Mean particle size | 0.60 | mm | 23.6 | μinch | 
| Particle density | 1.20 | kg/l | 78.6 | lb/ft³ | 
| Shipping weight | 0.80 | kg/l | 50 | lb/ft³ | 
| Maximum work temperature | 120 | °C | 250 | °F | 
| PH range | 0-14 | |||
| Min. bed depth | 800 | mm | 2.6 | ft | 
| Service flow rate | 5-60 | m/h | 2-24 | gpm/ft2 | 
| Co-current regeneration rinse | 1-10 | m/h | 0.4-4 | gpm/ft2 | 
| Counter-current regeneration rinse | 5-20 | m/h | 2-8 | gpm/ft2 | 
| Total rinse requirement | 2-5 bed volumes | |||
| Regenerant | NaCl (8-12%) | |||