| Thermoplastic | ||||
| Polyimide (PI) | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.38 *10³ | kg/m³ | 86.1 | lb/ft³ | 
|---|---|---|---|---|
| Modulus of elasticity | 3.1 | GPa | 440 | ksi | 
| Tensile strength | 96 | MPa | 14000 | psi | 
| Elongation | 7 | % | 7 | % | 
| Flexural strength | 143 | MPa | 21000 | psi | 
| Thermal expansion (20 ºC) | 43*10-6 | ºCˉ¹ | 24*10-6 | in/(in* ºF) | 
| Thermal conductivity | 0.40 | W/(m*K) | 2.77 | BTU*in/(hr*ft²*ºF) | 
| Glass transition temperature | 320 | ºC | 608 | ºF | 
| Maximum work temperature | 380 | ºC | 720 | ºF | 
| Dielectric constant | 3.5 | - | 3.5 | - | 
Applications: aerospace components, high temperature resistant foams, chemical fibers, arc welding torches.