Two component fast curing epoxy adhesive | ||||
Two component, clear, non-yellowing fast curing epoxy adhesive | ||||
Property | Value in metric unit | Value in US unit | ||
Viscosity (mixed) at 77°F (25°C) | 12000 | cP | 0.251 | lbf*sec/ft² |
---|---|---|---|---|
Working strength time | 5 | min | 5 | min |
Full cure time | 24 | hrs | 24 | hrs |
Maximum gap | 2 | mm | 0.08 | in |
Shear strength, steel-to-steel 77°F (25°C) | 13 | MPa | 1885 | psi |
Peel strength, steel-to-steel 77°F (25°C) | 45 | N/(25mm width) | 10 | PIW (lbf/inch width) |
Min. service temperature | -40 | ºC | -40 | ºF |
Max. service temperature | 80 | ºC | 175 | ºF |