| UV cure thixotropic urethane adhesive | ||||
| UV cure thixotropic single component electrically insulating urethane adhesive | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.02 *10³ | kg/m³ | 68.7 | lb/ft³ | 
|---|---|---|---|---|
| Viscosity | thixotropic paste | |||
| Hardness, Durometer A | 80 | A | 80 | A | 
| Solids | 100 | % | 100 | % | 
| Glass transition temperature | -60 | ºC | -76 | ºF | 
| Thermal expansion (20 ºC) | 2.4*10-4 | ºCˉ¹ | 1.3*10-4 | in/(in* ºF) | 
| Volume resistivity | 5.4*1014 | ohm*cm | 2.1*1014 | ohm*in | 
| Dielectric strength, 0.003” film | > 60 | KV/mm | > 1500 | V/mil | 
| Dielectric constant (1kHz) | 3.5 | 3.5 | ||
| Dissipation factor (1kHz) | 0.03 | 0.03 | ||
| Insulation resistance | 1*1013 | ohm | 1*1013 | ohm |