Mineral based oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 1.005 *10³ kg/m³ 62.7 lb/ft³
Kinematic viscosity at 104°F (40°C) 27.3 cSt 27.3 cSt
Flash point 232 ºC 450 ºF
Pour Point -25 ºC -13 ºF


Applications: machining of steels: drilling, milling, threading, broaching, boring, turning, tapping, engraving, reaming and sawing.