 Annealing is a heat treatment procedure involving heating the alloy and holding it at a certain temperature (annealing temperature), followed by controlled cooling.
Annealing results in relief of internal stresses, softening, chemical homogenizing and transformation of the grain structure into more stable state.
Annealing increases an extent of equilibrium of the metal structure resulting in softening and high ductility.
Annealing temperature and the control cooling rate depend on the alloy composition and the type of the annealing treatment.
The following types of annealing are used in heat treatment of alloys:
For the non-ferrous alloys full annealing means full softening after cold work in contrast to partial annealing meaning partial softening.
Recrystallization annealing is widely used as an intermediate softening treatment between stages of cold work (cold rolling, drawing).
Combination of recrystallization annealing and cold work allows to control the microstructure grains size.
The stress relief temperature is lower than the recrystallization temperature.
This treatment improves the machining characteristics of the steel.
Homogenizing annealing is used for steel and aluminum ingots and castings.
More homogeneous intercrystalline distribution of carbon, phosphorus sulfur and alloying elements in steel ingots is achieved in annealing at 2000°F -2370°F (1100°C - 1300°C) for 20-50 hrs.
Aluminum alloys are treated at 790°F - 970°F (420°C - 520°C) for 16-30 hrs. 
 