| Carbon-Carbon Composite (uni-directional fibers) | ||||
| Composition: carbon matrix + carbon fibers | ||||
| Property | Value in metric unit | Value in US unit | ||
| Modulus of elasticity | 135 | GPa | 19600 | psi | 
|---|---|---|---|---|
| Tensile strength | 650 | MPa | 94300 | psi | 
| Compressive strength | 650 | MPa | 94300 | psi | 
| Fracture energy | 1.7 | kJ/m2 | 0.15 | BTU/ft2 | 