Paint is a coating applied to the surface in form of a liquid dispersion, which is then hardens forming a solid film.

The functions of paints:

  • Protection of the part surface from the environmental factors (Oxygen and other chemically active gases, moisture, dissolved salts and other chemicals, temperature, bacteria, fungi). Corrosion protection is the most important function of paints.
  • Aesthetic appearance provided by the paint color and sheen (eggshell, satin or gloss).
  • Providing a desired ability of reflection-absorption of heat and light.
  • Changing the surface properties: ant-friction, hardness, electrical conductivity.
  • Identification of products according to the color of the paint.

Classification of paints:

Classification of paints by physical type

  • Solvent-borne paints contain up to 80% of solid constituents (binders, pigments and additives) dispersed in the organic solvent. Solvent-borne paints dry fast and may contain a wide range of binders. The main disadvantages of the solvent-borne paints are their toxicity and combustibility.
  • Water-borne paints contain water as the paint solvent. Waterborne paints are non-toxic and non-combustible but they are characterized by long drying time due to slow evaporation rate of water.
  • High-solids paints (Low VOC paints) contain more than 80% of solid constituents (binders, pigments) dispersed in an organic solvent. VOC - volatile organic compounds.
  • Powder coatings are obtained from powdered resin, particles of which are attracted by the electrostatic force to the substrate surface (electrodeposition). No solvent is involved in the process therefore powder coatings produce no/low toxic waste. The main disadvantage of powder coatings is high cost of equipment.
  • Radiation curable coatings are formed from a mixture of prepolymers, monomers and additives, which is cured under ultra-violet radiation. Radiation curable coatings harden fast and contain no solvents. The main disadvantage is relatively high cost.

to top

Classification of painting products by their functions

  • Paint - colored non-transparent protective coating.
  • Varnish - transparent or semi-transparent protective coating. A varnish is made of binder, solvent and additives. Some varnishes contain small amounts of pigment.
  • Enamel - hard protective coating with glossy finish.
  • Primer - the first coating applied to the surface in order to enhance the adhesion of the final paint (topcoat) and to seal the substrate surface. Primer may be formulated to impart additional protection to the substrate (eg. anti-rust primer for steel substrates).

to top


Related internal links

classification_of_paints.txt ยท Last modified: 2023/12/13 by dmitri_kopeliovich
Promote in SubsTech       Creative Commons License Except where otherwise noted, this work is licensed under a Creative Commons Attribution-Noncommercial-Share Alike 3.0 License