| Compressor oil ISO 68 | ||||
| Mineral based oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.871 *10³ | kg/m³ | 54.4 | lb/ft³ | 
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 67.4 | cSt | 67.4 | cSt | 
| Kinematic viscosity at 212°F (100°C) | 8.9 | cSt | 8.9 | cSt | 
| Viscosity index | 104 | 104 | ||
| Flash point | 244 | ºC | 471 | ºF | 
| Pour Point | -15 | ºC | 5 | ºF | 
| Color | 0.5 | 0.5 | ||
| NOACK volatility (weigh loss) | 12.02 | % | 12.02 | % | 
Applications: screw compressors.