| Elastomer | ||||
| Nitrile | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.0 *10³ | kg/m³ | 62.4 | lb/ft³ | 
|---|---|---|---|---|
| Tensile strength | 28 | MPa | 4060 | psi | 
| Elongation | 700 | % | 700 | % | 
| Glass transition temperature | -55 | ºC | -67 | ºF | 
| Maximum work temperature | 100 | ºC | 212 | ºF | 
| Electric resistivity | 102 | Ohm*m | 104 | Ohm*cm | 
| Dielectric constant | 13 | - | 13 | - | 
Applications: hoses, gaskets, tanks lining, rolls coating.