| Gear oil SAE 80W-90 | ||||
| Mineral based multigrade gear oil | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density at 60°F (15.6°C) | 0.887 *10³ | kg/m³ | 55.4 | lb/ft³ | 
|---|---|---|---|---|
| Kinematic viscosity at 104°F (40°C) | 139 | cSt | 139 | cSt | 
| Kinematic viscosity at 212°F (100°C) | 15 | cSt | 15 | cSt | 
| Viscosity index | 110 | 110 | ||
| Brookfield viscosity at -14.8°F (-26°C) | 136000 | cP | 136000 | cP | 
| Flash point | 218 | ºC | 424 | ºF | 
| Pour Point | -27 | ºC | -16.6 | ºF | 
| Channel Point | max.-35 | ºC | max.-31 | ºF | 
| Color | 2.5 | 2.5 | ||