| High strength compression molded carbon-graphite | ||||
| Chemical composition: carbon (C) | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 1.7*10³ | kg/m³ | 106 | lb/ft³ | 
|---|---|---|---|---|
| Porosity | 11 | % | 11 | % | 
| Flexural strength | 55 | MPa | 7980 | psi | 
| Compressive strength | 155 | MPa | 22475 | psi | 
| Hardness | 85 | scleroscope | 85 | scleroscope | 
| Thermal expansion (20 ºC) | 3*10-6 | ºCˉ¹ | 1.7*10-6 | in/(in* ºF) | 
| Thermal conductivity | 120 | W/(m*K) | 832 | BTU*in/(hr*ft²*ºF) | 
| Max. service temperature | 399 | °C | 750 | ºF | 
 Applications: bearings, bushings.