| Silver-ABA | ||||
| Chemical composition: Ag=92.75%, Cu=5.0%, Ti=1.25%, Al-1.0% | ||||
| Property | Value in metric unit | Value in US unit | ||
| Density | 10.0 *10³ | kg/m³ | 5.27 | Troy oz/in³ | 
|---|---|---|---|---|
| Modulus of elasticity | 77 | GPa | 11170 | ksi | 
| Thermal expansion (20 ºC) | 2.07*10-5 | ºCˉ¹ | 1.15*10-5 | in/(in* ºF) | 
| Thermal conductivity | 344 | W/(m*K) | 2385 | BTU*in/(hr*ft²*ºF) | 
| Electrical resistivity | 2.2*10-8 | Ohm*m | 2.2*10-6 | Ohm*cm | 
| Tensile strength | 136 | MPa | 20000 | psi | 
| Yield strength | 282 | MPa | 41000 | psi | 
| Elongation | 37 | % | 37 | % | 