Polyalphaolefin synthetic multigrade engine oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.865 *10³ kg/m³ 54.0 lb/ft³
Kinematic viscosity at 104°F (40°C) 57.6 cSt 57.6 cSt
Kinematic viscosity at 212°F (100°C) 10.6 cSt 10.6 cSt
Viscosity index 175 175
CCS viscosity at -22°F (-30°C) 3950 cP 3950 cP
Flash point 218 ºC 424 ºF
Pour Point max. -46 ºC max. -51 ºF
Sulfated ash 0.9 % 0.9 %
Neutralization No. (TBN-E) 12.2 12.2
Color 2.3 2.3

Related internal links