White spirit

(submitted by the website administration)

White spirit
White spirit, Stoddard solvent
Property Value in metric unit Value in US unit
Density at 68°F (20°C) 0.78 *10³ kg/m³ 48.7 lb/ft³
Viscosity at 68°F (20°C) 1.2 cP 8*10-4 lb/ft·s
Vapor pressure at 77°F (25°C) 4.5 torr 4.5 torr
Boiling point 150-220 ºC 302-437 ºF
Flash Point 31-54 ºC 88-129 ºF
Autoignition temperature 240 ºC 464 ºF