Cast copper alloy C94300 (Soft Bronze) | ||||
Chemical composition: Sn=5.3%, Pb=25.0%, Cu=69.7% | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 9.30 *10³ | kg/m³ | 581 | lb/ft³ |
---|---|---|---|---|
Modulus of elasticity | 72.4 | GPa | 10500 | ksi |
Specific heat capacity | 377 | J/(kg*K) | 0.090 | BTU/(lb*ºF) |
Thermal conductivity | 62.7 | W/(m*K) | 434 | BTU*in/(hr*ft²*ºF) |
Electric resistivity | 18.9*10-8 | Ohm*m | 18.9*10-6 | Ohm*cm |
Tensile strength (sand cast) | 186 | MPa | 27000 | psi |
Yield strength (sand cast) | 90 | MPa | 13000 | psi |
Elongation (sand cast) | 15 | % | 15 | % |
Hardness (sand cast) | 48 | HB(500) | 48 | HB(500) |