Pt 950/Ir | ||||
Chemical composition: 95% Pt, 5% Ir | ||||
Property | Value in metric unit | Value in US unit | ||
Density | 21.51 *10³ | kg/m³ | 1343 | lb/ft³ |
---|---|---|---|---|
Specific heat capacity | 126 | J/(kg*K) | 0.03 | BTU/(lb*ºF) |
Thermal conductivity | 75 | W/(m*K) | 520 | BTU*in/(hr*ft²*ºF) |
Heat of fusion | 1.187*105 | J/kg | 51.03 | BTU/lb |
Elongation (annealed) | 30 | % | 30 | % |
Hardness (annealed) | 80 | HV | 80 | HV |
Liquidus temperature | 1795 | ºC | 3263 | ºF |