Way lubricant ISO 220
Mineral based oil
Property Value in metric unit Value in US unit
Density at 60°F (15.6°C) 0.896 *10³ kg/m³ 55.9 lb/ft³
Kinematic viscosity at 104°F (40°C) 241 cSt 241 cSt
Kinematic viscosity at 212°F (100°C)/) 20.8 cSt 20.8 cSt
Viscosity index 96 96
Flash point 288 ºC 550 ºF
Pour Point -12 ºC -10 ºF
Total acid No. 1.15 1.15
Color 4.5 4.5